TABOREN-PC 51 H 20-851 is a compound based on polypropylene copolymer filled with 20% of hybrid filler (talc + glass fiber), stabilized with a standard and UV antioxidant package. It is designed for injection molding technology and used in many industrial fields with stress put on excellent processability and good surface performance.Information provided by Silon US LLC. |