MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Momentive Performance Materials GE Silicones Enduris 3500 Silicone Roof Coating
Categories: Polymer; Thermoset; Silicone

Material Notes: GE Enduris 3500 silicone roof coating is a high performing protective barrier for a variety of architectural surfaces and roofing substrates. Upon cure, Enduris 3500 silicone roof coating forms a durable, breathable and weatherproof roofing membrane that is highly resistant to degradation from UV and natural weathering.

Features: Silicone Durability, VOC Compliant, Ease of Use, Versatile Application, High Build Formulation, Storage & Shelf Life.

Applications: For structurally sound roofing applications including over existing coatings, single ply, modified bitumen and BUR, foam, metal and other horizontal and vertical roofing. Perform an adhesion test on each surface type to ensure adhesion.

Information provided by Momentive Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Solids Content 90 %By volume.; ASTM D1644-01 (Modified)
 91 %By weight.; ASTM D1644-01 (Modified)
Volatile Organic Compounds (VOC) Content <= 24 g/lEPA Method 24
Viscosity 22000 cPASTM D2196
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 36ASTM D2240
Tensile Strength 1.41 MPaASTM D2370
Elongation at Break 540 %ASTM D2370
Tear Strength 5.71 kg(f)/cmASTM D624
 
Optical PropertiesOriginal ValueComments
Emissivity (0-1) 0.89Enduris 3502 (white). Aged.; ASTM C1371
 0.90Enduris 3502 (white). Initial.; ASTM C1371
Reflection Coefficient, Visible (0-1) 0.55Solar Reflectance; Enduris 3502 (white); Aged; ASTM C1549
 0.88Solar Reflectance; Enduris 3502 (white); ASTM C1549
 
Processing PropertiesOriginal ValueComments
Tack-Free Time 20.0 - 30.0 minASTM D3960
 
Descriptive Properties
ColorWhite, tan, protection yellow, light gray, medium gray, black
Low Temperature FlexibilityPassASTM D522 (B).
Resistance to Wind Driven RainpassTT-C-555B
Skin Over Time10-15 minutesWPSTM C-560
SRI Value111ASTM E1980. Enduris 3502 (white). Initial.
 65ASTM E1980. Enduris 3502 (white). Aged.
Water Vapor Permeance9.3 permsASTM E96 (BW).

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMOMEN9909 / 265718

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.