MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Aremco

Aremco Ceramacast™ 900 High Temperature Potting & Casting Material Zirconia Silicate  (discontinued **)
Categories: Ceramic; Oxide; Silicon Oxide; Zirconium Oxide

Material Notes: High Density, high strength molding compound.

Vendors: Aremco’s Ceramacast casting and potting compounds represent the most expansive line of products based on aluminum oxide, aluminum nitride, magnesium oxide, silicon dioxide, silicon carbide, zirconium oxide, and zirconium silicate for applications to 3000°F (1760°C). Visit us today at Aremco.com or call 1 (845) 268-0039 to speak with an engineer.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Bulk Density 1.56 g/cc0.0562 lb/in³Powder
Porosity <= 5.0 %<= 5.0 %
pH 5.0 - 6.05.0 - 6.0
Viscosity 25000 cP25000 cP
 
Mechanical PropertiesMetricEnglishComments
Compressive Strength 55.2 MPa8000 psi
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+9 ohm-cm1.00e+9 ohm-cm
Dielectric Strength 4.92 kV/mm125 kV/in
 
Thermal PropertiesMetricEnglishComments
CTE, linear 5.04 µm/m-°C
@Temperature 20.0 °C
2.80 µin/in-°F
@Temperature 68.0 °F
Maximum Service Temperature, Air 1540 °C2800 °F
Shrinkage <= 1.0 %
@Temperature 538 °C
<= 1.0 %
@Temperature 1000 °F
 
Processing PropertiesMetricEnglishComments
Dry Time >= 8 hour>= 8 hourAir dry
Cure Time 300 - 420 min5.00 - 7.00 hour2-4 hrs at 200°F; 3 hrs at 250°F
Pot Life <= 20 min<= 20 min
Shelf Life 12.0 Month12.0 Month
 
Descriptive Properties
Acid ResistanceGood
Alkali ResistanceGood
ColorOff White
Mix Ratio100:15-17
Moisture ResistanceGood

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aremco Ceramacast™ 646-N High Temperature Potting & Casting Material Zirconia
Aremco Ceramacast™ 895 High Temperature Potting & Casting Material Alumina
Aremco Ceramacast™ 673-N High Temperature Potting & Casting Material Silicon Carbide
Aremco Ceramacast™ 586 High Temperature Potting & Casting Material Zirconia Silicate
Aremco Ceramacast™ 510 High Temperature Potting & Casting Material Alumina

ZCAREM46a / 138301

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.