MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Syensqo (Solvay Specialty Polymers) Ryton® R-4-242NA Polyphenylene Sulfide (PPS), 40% Glass Fiber  (discontinued **)
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS); Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler

Material Notes: Ryton® R-4-242NA 40% glass fiber reinforced polyphenylene sulfide compound complies with United States Food and Drug Administration (FDA) and European Union (EU 10/2011 and 1183/2012) regulations for use as a component of articles intended for repeat use in contact with all types of foods.

Key Attributes: Food Contact Acceptable

Applications: Appliance Components

Agency Ratings: AAMA 303; ACS Unspecified Rating; DVGW W270; EU 10/2011; FDA Food Contact, Unspecified Rating; KTW Unspecified Rating; NSF STD-61; WRAS Unspecified Rating

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.68 g/cc0.0607 lb/in³ASTM D792
Water Absorption 0.014 %
@Time 86400 sec
0.014 %
@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0020 cm/cm
@Thickness 3.20 mm
0.0020 in/in
@Thickness 0.126 in
ASTM D255
Linear Mold Shrinkage, Transverse 0.0050 cm/cm
@Thickness 3.20 mm
0.0050 in/in
@Thickness 0.126 in
ASTM D255
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 103103ASTM D785
Hardness, Rockwell R 123123ASTM D785
Tensile Strength 190 MPa27600 psiASTM D638
Elongation at Break 1.7 %1.7 %ISO 527-2
Tensile Modulus 15.1 GPa2190 ksiISO 527-2
Flexural Strength 270 MPa39200 psiISO 178
Flexural Modulus 14.7 GPa2130 ksiISO 178
Compressive Strength 270 MPa39200 psiASTM D695
Poissons Ratio 0.390.39ASTM E132
Izod Impact, Notched 0.850 J/cm
@Thickness 3.18 mm
1.59 ft-lb/in
@Thickness 0.125 in
ASTM D256
Izod Impact, Unnotched 6.40 J/cm
@Thickness 3.18 mm
12.0 ft-lb/in
@Thickness 0.125 in
ASTM D256
Izod Impact, Notched (ISO) 10.0 kJ/m²4.76 ft-lb/in²Notch A; ISO 180
 11.0 kJ/m²
@Temperature -40.0 °C
5.23 ft-lb/in²
@Temperature -40.0 °F
ISO 180
Izod Impact, Unnotched (ISO) 36.0 kJ/m²17.1 ft-lb/in²ISO 180
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.50e+16 ohm-cm1.50e+16 ohm-cmASTM D257
Surface Resistance 5.20e+15 ohm5.20e+15 ohmASTM D257
Dielectric Constant  3.49
@Frequency 1000 Hz
3.49
@Frequency 1000 Hz
ASTM D150
 3.49
@Frequency 1e+6 Hz
3.49
@Frequency 1e+6 Hz
ASTM D150
Dissipation Factor  0.0010
@Frequency 1000 Hz
0.0010
@Frequency 1000 Hz
ASTM D150
 0.0020
@Frequency 1e+6 Hz
0.0020
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  11.0 µm/m-°C
@Temperature 125 - 200 °C
6.11 µin/in-°F
@Temperature 257 - 392 °F
ASTM E831
 14.0 µm/m-°C
@Temperature -50.0 - 50.0 °C
7.78 µin/in-°F
@Temperature -58.0 - 122 °F
ASTM E831
 14.0 µm/m-°C
@Temperature 50.0 - 100 °C
7.78 µin/in-°F
@Temperature 122 - 212 °F
ASTM E831
CTE, linear, Transverse to Flow  42.0 µm/m-°C
@Temperature -50.0 - 50.0 °C
23.3 µin/in-°F
@Temperature -58.0 - 122 °F
ASTM E831
 51.0 µm/m-°C
@Temperature 50.0 - 100 °C
28.3 µin/in-°F
@Temperature 122 - 212 °F
ASTM E831
 110 µm/m-°C
@Temperature 125 - 200 °C
61.1 µin/in-°F
@Temperature 257 - 392 °F
ASTM E831
Thermal Conductivity 0.310 W/m-K2.15 BTU-in/hr-ft²-°FASTM C177
Melting Point 285 °C545 °F
Deflection Temperature at 1.8 MPa (264 psi) 268 °C514 °FUnannealed; ASTM D648
Flammability, UL94 V-0V-0UL 94
 
Descriptive Properties
Availability (as of March 2019)Asia Pacific; Europe; Latin America; North America
ColorNatural Color
FormsPellets
ProcessingInjection Molding
RoHS ComplianceRoHS Compliant

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSOL8Y5318 / 238699

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.