Description: - Thin, flexible, resonant-tuned, lightweight foam absorber.
- SS-11410 is based on the quarter wavelength principle which assures effective cancellation of the incident wave at the front of the absorber.
- Available with pressure sensitive adhesive (PSA).
- Can be water-jet or die cut for custom configurations.
- Halogen free, RoHS and REACH compliant.
Information provided by Hexcel Corporation. |