MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Thermal Ceramics TC-26 High Temperature Insulating Firebrick
Categories: Ceramic

Material Notes: The bond developed is a ceramic bond that is formed by high temperature firing. This produces bricks that are very stable and strong at temperatures higher than 2600°F (1427°C).

Features:

  • High temperature insulating firebrick with use limits up to 3250°F (1788°C)
  • Excellent strength and thermal stability
  • Low heat storage
  • High purity
  • Excellent thermal conductivity
  • Applications:

  • Atmosphere furnace
  • Forge furnaces
  • Ethylene furnace sidewalls
  • Ceramic kilns
  • High temperature back-up insulation
  • Carbon baking furnaces
  • High temperature kiln linings
  • Removable furnace doors
  • Information provided by Thermal Ceramics

    Data has not been recently verified. Please contact manufacturer for current information.

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesMetricEnglishComments
    Density 0.769 g/cc0.0278 lb/in³
    Deformation 0.20 %0.20 %at 10 psi; 1.5 hours at 2200°F
     
    Mechanical PropertiesMetricEnglishComments
    Modulus of Rupture 0.00138 GPa0.200 ksi
    Compressive Strength 1.86 MPa270 psi
     
    Thermal PropertiesMetricEnglishComments
    Thermal Conductivity  0.231 W/m-K
    @Temperature 260 °C
    1.60 BTU-in/hr-ft²-°F
    @Temperature 500 °F
    ASTM C201
     0.274 W/m-K
    @Temperature 538 °C
    1.90 BTU-in/hr-ft²-°F
    @Temperature 1000 °F
    ASTM C201
     0.317 W/m-K
    @Temperature 816 °C
    2.20 BTU-in/hr-ft²-°F
    @Temperature 1500 °F
    ASTM C201
     0.375 W/m-K
    @Temperature 1090 °C
    2.60 BTU-in/hr-ft²-°F
    @Temperature 2000 °F
    ASTM C201
    Maximum Service Temperature, Air 1430 °C2600 °F
    Shrinkage -0.100 %
    @Temperature 1400 °C,
    Time 86400 sec
    -0.100 %
    @Temperature 2550 °F,
    Time 24.0 hour
     
    Component Elements PropertiesMetricEnglishComments
    Al2O3 47 %47 %
    Alkalis 2.0 %2.0 %
    CaO 0.30 %0.30 %
    Fe2O3 0.70 %0.70 %
    MgO 0.10 %0.10 %
    SiO2 48.6 %48.6 %
    TiO2 1.3 %1.3 %

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

    Users viewing this material also viewed the following:
    Thermal Ceramics Firebrick SR-99
    Thermal Ceramics Firebrick SR-90
    China-Yixing Longly Refractories ASM-130 Cordierite-Mullite
    Thermal Ceramics Firebrick SR-99 LS
    China-Yixing Longly Refractories ASM-120 Cordierite-Mullite

    CTHERM127 / 2447

    Free Trade Publications, Click Here!
    Free Trade Publications, Click Here!

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.