MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
BCC Products BC 4558 Polyester Filler Paste
Categories: Polymer; Thermoset; Polyester, TS

Material Notes: BC4558 is a unique quickset paste designed for aircraft use in making fast repairs to damaged metal surfaces. Also recommended for use in edge filling honeycomb core and foam core composite panels. BC4558 features the following: 1. Quick setting, tack-free cure, 2. Fire resistant, 3. Light-bodied consistency, 4. Highly thixotropic, excellent vertical sag resistance, 5. Semi-resilient cure to withstand vibration, 6. Excellent sanding and finishing properties

Information provided by BCC Products, Inc.

Key Words: Fire Retardant
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.900 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 72
Tensile Strength, Ultimate 1220 psi
Flexural Strength 2480 psi
Compressive Strength 4900 psi
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 118 °F
Flammability Test 100HLT-15
 
Processing PropertiesOriginal ValueComments
Cure Time 30.0 min
@Temperature 24.0 °C
Gel Time 6.0 - 10 min
@Temperature 24.0 °C
Shelf Life 6.00 Monthin tightly closed container
 
Descriptive Properties
Flammability Test ()passes F.A.R. 25.853
Mix Ratio100:2 resin/hardener
Mixed Viscosity, BrookfieldThixotropic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PBCC003 / 107230

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.