MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

Ensinger TECAMID 66 HI natural Nylon 66
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Unreinforced

Material Notes:
  • heat stabilized
  • low thermal expansion
  • good mechanical properties
  • good dimensional stability
Target Industries:
  • conveyor technology
  • heavy duty industry
  • mechanical engineering
  • power engineering

Information provided by Ensinger Inc.

Vendors: Ensinger High Performance Plastics withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.15 g/cc0.0415 lb/in³
Moisture Absorption 0.275 %
@Time 86400 sec
0.275 %
@Time 24.0 hour
ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 68.9 MPa10000 psiASTM D 638
Elongation at Break 25 %25 %ASTM D 638
Modulus of Elasticity 2.41 GPa350 ksiASTM D 638
Flexural Modulus 3.03 GPa440 ksiASTM D 790
Izod Impact, Unnotched 0.641 J/cm1.20 ft-lb/inASTM D 256
 
Thermal PropertiesMetricEnglishComments
Melting Point 262 °C504 °FASTM D 2133
Maximum Service Temperature, Air 85.0 °C185 °FLong Term
Deflection Temperature at 0.46 MPa (66 psi) 200 °C392 °FASTM D 648
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °C194 °FASTM D 648
Flammability, UL94 HBHB
 
Descriptive Properties
Colornatural opaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PENSIN8169 / 319097

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.