MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Covestro Makrolon® DP 1-1456 Polycarbonate, Impact Grade  (discontinued **)
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Impact Modified

Material Notes: Impact modified injection molding grade, extremely easy flow and easy mold release, for thin walled applications with long flow lengths.

Information provided by Bayer.

As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.

Key Words: PC
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.20 g/cc
Moisture Absorption at Equilibrium 0.15 %50% RH
Water Absorption at Saturation 0.35 %
 0.35 %
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cmASTM D955
Melt Flow 27 g/10 min
@Load 1.20 kg,
Temperature 300 °C
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 55.0 MPaASTM D638
Tensile Strength, Yield 55.0 MPa
Elongation at Break >= 50 %Nominal
Elongation at Yield 5.5 %
Tensile Modulus 2.00 GPa
Flexural Yield Strength 83.0 MPaat 5% strain; ASTM D790
Flexural Modulus 2.10 GPaASTM D790
Izod Impact, Notched 5.87 J/cm
@Thickness 3.20 mm
ASTM D256
Charpy Impact Unnotched NB
Impact Test 65.0 J
@Thickness 3.20 mm
Instrumented total energy; 3.2 mm thick; 0.5 in. dart; 3 in. clamp; 15 mph; ASTM D3763
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 135 °C
Deflection Temperature at 1.8 MPa (264 psi) 123 °C
Vicat Softening Point 144 °C
UL RTI, Electrical 80.0 °C
@Thickness 1.50 mm
UL RTI, Mechanical with Impact 80.0 °C
@Thickness 1.50 mm
UL RTI, Mechanical without Impact 80.0 °C
@Thickness 1.50 mm
Flammability, UL94 HB
@Thickness 1.60 mm
(Black)
 
Processing PropertiesOriginal ValueComments
Melt Temperature 293 - 332 °C

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Mitsubishi Xantar® MX 1002 Polycarbonate
Mitsubishi Xantar® MX 1001 Polycarbonate
Mitsubishi Xantar® E EM 605 Polycarbonate
Mitsubishi Iupilon® GPX 2010PH Polycarbonate
LG Chemical LUPOY SC1004AU PC, High Impact

PBA462 / 26963

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.