MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Goodfellow T1-Thermocouple Alloy
Categories: Metal; Electronic/Magnetic Alloy; Nonferrous Metal; Nickel Alloy

Material Notes: The positive element of the type K thermocouple alloy the negative being T2. The thermocouple can be used up to 1250C in oxidizing atmospheres and is the probably the most common in use. It is also the positive element of the type E thermocouple with Constantan as the negative; the thermoelectric power of type E thermocouples is the highest amongst all standard couples

Information provided by Goodfellow.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.50 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 620 - 780 MPa
Elongation at Break <= 44 %
Modulus of Elasticity 186 GPa
Izod Impact, Unnotched 1.08 J/cmNotch Status Unknown
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000706 ohm-cmTemperature Coefficient of 0.00032/K
 
Thermal PropertiesOriginal ValueComments
CTE, linear 17.2 µm/m-°C
@Temperature 20.0 - 1000 °C
Thermal Conductivity 19.0 W/m-K
Melting Point 1420 °C
Maximum Service Temperature, Air 1100 °C
 
Component Elements PropertiesOriginal ValueComments
Chromium, Cr 10 %
Nickel, Ni 90 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Constantan Thermocouple Wire
Hoskins Manufacturing Chromel® Thermocouple Wire
Goodfellow Manganin® Copper Resistance Alloy
Sandvik Iron Thermocouple
Sandvik Nicrosil Thermocouple

NGOODF226 / 16283

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.