Ducorit® R and A product lines are based on innovative ultra high performance cementitious technology that was developed in house by Densit® for use in structural grouted connections for wind turbine foundations and concrete tower joints. UHPC and HPC Densit® Technology. The differentproperties of Ducorit® A2G and Ducorit® R5G are obtained by a unique mix of high quality cement, aggregates and additives. The products are manufactured as ready-to-mix grout, in 25 kg to 1000 kg bags. Ducorit® products are characterized by extreme strength and high stiffness making Ducorit® a strong structural component, meeting international high design standards.Information provided by ITW Performance Polymers. |