MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Verdant Specialty Solutions MACKAM® MEJ Surfactant
Categories: Fluid; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Product Description: Mackam MEJ is an amphoteric wetting agent produced from caprylic imidazoline. It is stable in high alkaline systems, compatible with phosphate builders and provides low, stable foam in formulations. Mackam MEJ effectively couples other surfactants into highly built hard surface cleanser and is a functional equivalent to SXS. When formulated in glass and hard surface cleaners Mackam MEJ is noted for its low film and streak properties.

Uses: All Purpose Cleaners, Glass Cleaners, Hard Surface Cleaners and Grill Cleaners

Information provided by Rhodia, Rhodia has been acquired by Solvay. Verdant Specialty Solutions was created through the purchase of Solvay's amphoteric and secondary surfactants business

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.10 - 1.15 g/cc0.0397 - 0.0415 lb/in³
Solids Content 33 - 35 %33 - 35 %Moisture Balance
pH 9.5 - 10.59.5 - 10.5
 
Optical PropertiesMetricEnglishComments
Gardner Color Number <= 7.0<= 7.0
 
Processing PropertiesMetricEnglishComments
Shelf Life 24.0 Month24.0 Month
 
Descriptive Properties
AppearanceClear Liquid
Caustic Solubility<25%
CompositionMethanol0.02
 Sodium Chloride5.2-5.8%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WRHOD208 / 137439

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.