HBG5724 is 20% GF reinforced PBT/ABS resin. HBG5724 has excellent mechanical strength, high chem-resistance and high shape resistance property. HBG5724 is mainly used in automobile parts, electric & electron parts, switch, office appliance, etc. Information provided by Shanghai Kumho Sunny Plastics co, Ltd |