Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Teknor Apex Sarlink® TPV 3790 Thermoplastic Vulcanizate
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes: Notes: Sarlink TPV 3790 is a high performance thermoplastic vulcanizate used in automotive and industrial applications. Sarlink TPV 3790 is a high hardness, UV resistant, RoHS compliant grade exhibition superior compression set and chemical resistance. This grade can be processed by injection molding, blow molding and extrusion.

Availability: Asia Pacific; Europe; Latin America; North America

Features: Good Adhesion; Good Colorability; Good Processability; Medium Heat Resistant; UV Resistant; Weather Resistant

Uses: Diaphragms; Gaskets; Outdoor Applications; Seals

RoHS Compliance: RoHS Compliant

Automotive Specifications: PSA Peugeot-Citroen B62 0300 version G Color: Black

Form: Pellets

Processing Method: Extrusion; Injection Molding; Blow Molding

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.950 g/cc0.0343 lb/in³ISO 1183
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9494Injection Molded; ISO 868
Hardness, Shore D 3232Injection Molded; ISO 868
Tensile Strength at Break 14.0 MPa2030 psiAcross Flow; ISO 37
Tensile Stress at Strain 7.03 MPa
@Strain 100 %
1020 psi
@Strain 100 %
Across Flow; ISO 37
Elongation at Break 750 %750 %Across Flow; ISO 37
Compression Set 62 %
@Temperature 70.0 °C,
Time 79200 sec
62 %
@Temperature 158 °F,
Time 22.0 hour
ISO 815
 
Processing PropertiesMetricEnglishComments
Processing Temperature 185 - 220 °C365 - 428 °FInjection
Rear Barrel Temperature 180 - 215 °C356 - 419 °FInjection
Middle Barrel Temperature 180 - 215 °C356 - 419 °FInjection
Front Barrel Temperature 180 - 215 °C356 - 419 °FInjection
Nozzle Temperature 187 - 220 °C369 - 428 °FInjection
Zone 1 180 - 200 °C356 - 392 °FExtrusion
Zone 2 180 - 205 °C356 - 401 °FExtrusion
Zone 3 187 - 210 °C369 - 410 °FExtrusion
Zone 4 187 - 210 °C369 - 410 °FExtrusion
Die Temperature 195 - 215 °C383 - 419 °FExtrusion
Mold Temperature 10.0 - 55.0 °C50.0 - 131 °FInjection
Screw Speed 100 - 200 rpm100 - 200 rpmInjection
 
Descriptive Properties
AppearanceOpaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Teknor Apex Sarlink® TPV 5165N Thermoplastic Vulcanizate

PTEKNQ1152 / 237643

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.