MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Redwood Plastics Redco™ 70A Polyurethane
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: Redco™ 70A offers high compression resistance and withstands heavier loads while maintaining gripping characteristics. Redco™ 70A excels when bonded to steel as an impact pad or wheel cover.

Standard Color: Green

Features: Strong, Oil Resistant, Abrasion Resistant, Impact Resistant

Typical Applications: Packaging system parts, feed system parts, shock pads, springs, seals, shock and vibration pads, washers, roll covers, rollers, carry over wheels, bumpers, wheels, flexible parts, impact pads, anti-vibration parts, wipers, etc.

Information provided by Redwood Plastics and Rubber

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.21 g/cc0.0437 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 67 - 7367 - 73
Tensile Strength 44.0 MPa6380 psi
Elongation at Break 500 %500 %
100% Modulus 3.80 MPa551 psi
300% Modulus 9.50 MPa1380 psi
Resilience 5555DIN
Tear Strength 18.1 kN/m103 pliTrouser
 57.3 kN/m327 pliAngle, Die C
Abrasion 1717[mm3], DIN, 10N
Compression Set 29 %29 %Method B
 
Descriptive Properties
ColorGreen

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PREDW025 / 296591

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.