Product Description: LL 3201 resins are LLDPE hexane copolymer film resins. Films made from LL 3201 resins have outstanding tensile, stiffness and toughness properties. These superior properties, along with good drawdown capability, permit usage in many demanding packing applications. Availability: Latin America, North America and South America Additive: - Antiblock: No
- Slip: No
- Processing Aid: Yes
- Thermal Stabilizer: Yes
Applications: - Freezer Film
- Grocery Sacks
- Heavy Duty Bags
- Merchandise Bags
Information provided by ExxonMobil Chemical |