MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

IDI Composites Ultrium™ STC® 4660 EMC Structural Thermoset Composites, 60% Carbon Fiber
Categories: Polymer; Thermoset; Carbon Fiber/Thermoset Composite

Material Notes:
  • Ultra-high stiffness to weight ratio
  • Carbon pre-preg compatibility
  • High strength to weight ratio
  • For complex geometric applications requiring performance optimized high stiffness and low weight

Information provided by IDI Composites.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.44 g/cc1.44 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 301 MPa43700 psiASTM D638
Tensile Modulus 38.0 GPa5510 ksiASTM D638
Flexural Strength 609 MPa88300 psiASTM D790
Flexural Modulus 36.0 GPa5220 ksiASTM D790
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg 150 °C302 °FTan Delta
 
Descriptive Properties
Reinforcement Length25 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PIDI904 / 249294

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.