MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

TTC Taita TAITAREX® 818K GPPS
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Extrusion Grade

Material Notes: Characteristics:
  • Extrusion Grade
  • The most state of the art from US NOVA CHEMICAL
  • Low Residual Monomer
  • Good Heat Resistance
  • Mold Dimension Stability
  • Good Transparency
  • Easy Processing
  • High M.W.
  • High strength
Applications:
  • OPS/PSP sheet applications.

Information provided by Taita Chemical Company, Limited

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.04 g/cc1.04 g/ccISO 1183
Melt Flow 2.4 g/10 min
@Load 5.00 kg,
Temperature 200 °C
2.4 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 5.30 MPa769 psi50 mm/min; ISO 527
Elongation at Break 2.0 %2.0 %50 mm/min; ISO 527
Izod Impact, Notched 0.186 J/cm0.349 ft-lb/inISO 180/1A
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 95.0 °C203 °FUnanneale; ISO 75A
Vicat Softening Point 105 °C
@Load 1.00 kg
221 °F
@Load 2.20 lb
120°C/hr; ISO 306
Flammability, UL94 HB
@Thickness 1.59 mm
HB
@Thickness 0.0625 in
 
Optical PropertiesMetricEnglishComments
Haze 0.50 %
@Thickness 2.80 mm
0.50 %
@Thickness 0.110 in
 
Descriptive Properties
Residual SM monomer200 ppm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTTC023 / 281543

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.