  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Aluminum Bronze D , UNS C61400, HR50 Temper, Rod
Categories: Metal; Nonferrous Metal; Copper Alloy; Bronze

Material Notes: Temper: Drawn and Stress Relieved

Fabrication Properties: Good Suitability – Gas Shielded Arc Welding, Coated Metal Arc Welding, Spot Weld, Seam Weld, Butt Weld, Capacity for Being Cold Worked, Capacity for Being Hot Formed; Fair Suitability – Brazing

Common Fabrication Processes: Blanking; Drawing; Forming and Bending; Heading and Roll Threading

Typical uses: Bolts; Nuts; Stringers; Threaded Members; Chutes for Abrasive Grains; Condenser Head Plates; Condenser Tube and Piping Systems; Corrosion Resistant Vessels; Heat Exchanger Tubes; Machine Parts; Mining Shovels; Piping Systems; Sea Water Piping; Seamless Tubing and Pipe; Structural Components; Tanks; Tube Sheets; Welded Pipe; Fasteners; Marine Hardware; Pressure Vessels; Protective Sheathing; Welded Tanks; Blending Chambers; Mixing Troughs

Applicable Specifications: Bar – FEDERAL QQ-C-450, SAE J463, SAE J461; Bolts – ASTM F468; Nuts – ASTM F467; Pipe – ASTM B608; Plate – ASTM B100, ASTM B432, FEDERAL QQ-C-450;; Plate & Sheet - for Pressure Vessels, Condensers & Heat Exchangers ASTM B171/B171M, for Pressure Vessels, Condensers & Heat Exchangers ASME SB171; Rod – SAE J461, SAE J463; Rod, Bar & Shapes - for Pressure Vessels, Condensers & Heat Exchangers ASTM B150/B150M, for Pressure Vessels, Condensers & Heat Exchangers ASME SB150; Screws – ASTM F468; Seamless Condenser Tube & Ferrule Stock – ASME SB111; Seamless Pipe and Tube – ASTM B315, ASME SB315; Shapes – SAE J461; SAE J463; Sheet – FEDERAL QQ-C-450, SAE J463, SAE J461; Sheet, Strip & Rolled Bar - Aluminum Bronze ASME SB169, ASTM B169/B169M; ; Strip – FEDERAL QQ-C-450, SAE J463, SAE J461; Studs – ASTM F468

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.89 g/cc0.285 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength  >= 483 MPa
@Thickness 50.8 mm
>= 70000 psi
@Thickness 2.00 in
for Standard
 >= 517 MPa
@Thickness 25.4 mm
>= 75000 psi
@Thickness 1.00 in
for Standard
 >= 552 MPa
@Thickness 12.7 mm
>= 80000 psi
@Thickness 0.500 in
for Standard
Elongation at Break  >= 30 %
@Thickness 25.4 mm
>= 30 %
@Thickness 1.00 in
for Standard
 >= 30 %
@Thickness 12.7 mm
>= 30 %
@Thickness 0.500 in
for Standard
 >= 30 %
@Thickness 50.8 mm
>= 30 %
@Thickness 2.00 in
for Standard
Tensile Modulus 117 GPa17000 ksi
Modulus of Rigidity 44.1 GPa6400 ksi
Poissons Ratio 0.330.33Calculated
Machinability 20 %20 %
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000123 ohm-cm0.0000123 ohm-cm14% IACS
 
Thermal PropertiesMetricEnglishComments
CTE, linear 16.2 µm/m-°C
@Temperature 20.0 - 300 °C
9.00 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.377 J/g-°C0.0900 BTU/lb-°F
Thermal Conductivity 5.62 W/m-K39.0 BTU-in/hr-ft²-°F
Melting Point 1041 - 1046 °C1905 - 1915 °F
Solidus 1041 °C1905 °F
Liquidus 1046 °C1915 °F
Annealing Point 607.2 - 899 °C1125 - 1650 °F
 
Processing PropertiesMetricEnglishComments
Hot-Working Temperature 788 - 927 °C1450 - 1700 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 6.0 - 8.0 %6.0 - 8.0 %
Copper, Cu 87.3 - 92.5 %87.3 - 92.5 %As Balance
Iron, Fe 1.5 - 3.5 %1.5 - 3.5 %
Lead, Pb <= 0.010 %<= 0.010 %
Manganese, Mn <= 1.0 %<= 1.0 %
Phosphorus, P <= 0.015 %<= 0.015 %
Zinc, Zn <= 0.20 %<= 0.20 %
 
Descriptive Properties
US EPA Registered AntimicrobialYes

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

MC61400x2 / 293022

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.