MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Akrochem AKROCHLOR™ L-63 Chlorinated Paraffins
Categories: Other Engineering Material

Material Notes: Product Description: Akrochlor chlorinated paraffins are a low cost source of halogen for flame retardant purposes (usually in concert with Sb2O3) and are compatible with most polymers (use resin product in EPDM for maximum compatibility). Grade selection is usually based on the best combination of chlorine content, viscosity, volatility and cost for the end-use product. Akrochlor chlorinated paraffins are available in a variety of grades, in both liquid (L-Grades) and resin (R-Grades) form. Akrochlor resin grades offer the highest chlorine content, but liquids are often used for the combination effect of plasticizer and flame retardant. Chlorinated hydrocarbons are also very resistant to microbial and fungi attack.

Information provided by Akrochem Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.40 g/cc
Viscosity 45000 cP
Saybolt Viscosity at 210°F 310 SUS
 
Component Elements PropertiesOriginal ValueComments
Chlorine, Cl 62 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PAKZCH244 / 315162

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.