MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SEKISUI SPI ALLEN® 5060WLG ASA/ABS Sheet
Categories: Polymer; Thermoplastic; ABS Polymer; ASA Polymer

Material Notes: ALLEN® 5060WLG is high impact ABS capped with ASA for UV protection and low to medium gloss finish.

ALLEN® 5060WLG has been tested under laboratory conditions and has achieved a UL94 HB rating at 0.060 in (1.52mm) and above and meets the requirements of Federal Motor Vehicle Safety Standard No. 302 (FMVSS 302).

Suggested Application:

  • Vehicle Exterior
  • Marine Parts
  • Radomes
  • Agriculture Equipment Exteriors
  • Construction Equipment Exteriors
  • Lift Boom Exteriors
Features:
  • Custom color matching
  • Excellent UV properties
  • Edge trim easily used into future orders
  • Low to medium gloss finish
  • Color and gloss retention

Information provided by SEKISUI KYDEX, LLC.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.03 g/cc1.03 g/ccASTM D792
Water Absorption 0.270 %0.270 %equilibrium; ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 93.093.0ASTM D785
Tensile Strength 42.0 MPa6090 psiASTM D638
Tensile Modulus 1.9098 GPa276.99 ksiASTM D638
Flexural Strength 63.4 MPa
@Strain 5.00 %
9200 psi
@Strain 5.00 %
ASTM D790
Flexural Modulus 1.99 GPa289 ksiASTM D790
Compressive Yield Strength 47.5 MPa6890 psiASTM D695
Bearing Yield Strength <= 177.2 MPa<= 25700 psiASTM D953
 30.3 MPa
@Strain 4.00 %
4390 psi
@Strain 4.00 %
ASTM D953
Shear Strength 39.2 MPa5690 psiASTM D732
Izod Impact, Notched  1.655 J/cm
@Temperature -29.0 °C
3.100 ft-lb/in
@Temperature -20.2 °F
ASTM D256
 2.835 J/cm
@Temperature 23.0 °C
5.311 ft-lb/in
@Temperature 73.4 °F
ASTM D256
Gardner Impact  24.7 J
@Temperature -29.0 °C
18.2 ft-lb
@Temperature -20.2 °F
Drop Dart Impact, GE; ASTM D5420
 46.1 J
@Temperature 23.0 °C
34.0 ft-lb
@Temperature 73.4 °F
Drop Dart Impact, GE; ASTM D5420
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 20.4 kV/mm518 kV/inoil; ASTM D149
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Transverse to Flow 97.7 µm/m-°C54.3 µin/in-°FASTM E831
Deflection Temperature at 0.46 MPa (66 psi) 96.2 °C205 °Fannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 91.0 °C196 °Fannealed; ASTM D648
Flammability, UL94 HB
@Thickness 1.52 mm
HB
@Thickness 0.0598 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSEKIS542 / 325282

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.