MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

SABIC NORYL™ Resin NH7010 Polyphenylene Ether + PS (PPE+PS) (Americas)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene + Polyphenylene Ether, Unreinforced

Material Notes: NORYL™ NH7010 resin is a non-reinforced blend of polyphenylene ether (PPE) + high impact polystyrene (HIPS) and exhibits an excellent balance of non-brominated, non-chlorinated flame retardance, high heat resistance, good flow, and low specific gravity for light weight parts. This injection moldable grade carries UL94 flame ratings of 5VA at 2mm and V0 at 1.5mm along with a UL746C Outdoor Suitability rating of F1. NORYL NH7010 resin is an excellent candidate for applications such as electrical enclosures and solar/PV junction boxes.

Features: Low Creep Sensitivity,Non-Chlorinated,Non-Brominated,High Flow

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.09 g/cc1.09 g/ccASTM D792
Density 1.09 g/cc0.0394 lb/in³ISO 1183
Moisture Absorption 0.0200 %0.0200 %Injection Molding
 0.0500 %0.0500 %23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.25 %0.25 %ISO 62-1
Viscosity 10 cP
@Load 5.00 kg,
Temperature 300 °C
10 cP
@Load 11.0 lb,
Temperature 572 °F
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0050 - 0.0080 cm/cm
@Thickness 3.20 mm
0.0050 - 0.0080 in/in
@Thickness 0.126 in
SABIC method
Melt Flow 10.1 g/10 min
@Load 5.00 kg,
Temperature 300 °C
10.1 g/10 min
@Load 11.0 lb,
Temperature 572 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 49.0 MPa7110 psi50 mm/min; ASTM D638
 63.0 MPa9140 psi50 mm/min; ISO 527
Tensile Strength, Yield 68.0 MPa9860 psi50 mm/min; ASTM D638
 69.0 MPa10000 psi50 mm/min; ISO 527
Elongation at Break 8.4 %8.4 %50 mm/min; ISO 527
 41 %41 %50 mm/min; ASTM D638
Elongation at Yield 4.9 %4.9 %50 mm/min; ISO 527
 5.2 %5.2 %50 mm/min; ASTM D638
Tensile Modulus 2.25 GPa326 ksi5 mm/min; ASTM D638
 2.50 GPa363 ksi1 mm/min; ISO 527
Flexural Strength 102 MPa14800 psiyld, 1.3 mm/min, 50 mm span; ASTM D790
 109 MPa15800 psiyield, 2 mm/min; ISO 178
Flexural Modulus 2.47 GPa358 ksi1.3 mm/min, 50 mm span; ASTM D790
 2.52 GPa365 ksi2 mm/min; ISO 178
Izod Impact Notched 223 J164 ft-lbASTM D256
 89.0 J
@Temperature -30.0 °C
65.6 ft-lb
@Temperature -22.0 °F
ASTM D256
Izod Impact, Notched (ISO) 20.0 kJ/m²9.52 ft-lb/in²80*10*4; ISO 180/1A
 8.00 kJ/m²
@Temperature -30.0 °C
3.81 ft-lb/in²
@Temperature -22.0 °F
80*10*4; ISO 180/1A
Charpy Impact, Notched 2.10 J/cm²9.99 ft-lb/in²Edgew 80*10*4 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 38.0 J28.0 ft-lbASTM D3763
 
Electrical PropertiesMetricEnglishComments
Arc Resistance 60 - 120 sec60 - 120 secASTM D495
Comparative Tracking Index 175 - 250 V175 - 250 VUL 746A
Hot Wire Ignition, HWI  30 - 60 sec
@Thickness >=1.50 mm
30 - 60 sec
@Thickness >=0.0591 in
UL 746A
 >= 120 sec
@Thickness >=3.00 mm
>= 120 sec
@Thickness >=0.118 in
UL 746A
High Amp Arc Ignition, HAI  30 - 60 arcs
@Thickness >=0.750 mm
30 - 60 arcs
@Thickness >=0.0295 in
UL 746A
 60 - 120 arcs
@Thickness >=1.50 mm
60 - 120 arcs
@Thickness >=0.0591 in
UL 746A
High Voltage Arc-Tracking Rate, HVTR >= 150 mm/min>= 5.91 in/minUL 746A
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  81.6 µm/m-°C
@Temperature -40.0 - 40.0 °C
45.3 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 81.6 µm/m-°C
@Temperature -40.0 - 40.0 °C
45.3 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow  81.5 µm/m-°C
@Temperature -40.0 - 40.0 °C
45.3 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 81.5 µm/m-°C
@Temperature -40.0 - 40.0 °C
45.3 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 139 °C282 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
 139 °C
@Thickness 3.20 mm
282 °F
@Thickness 0.126 in
unannealed; ASTM D648
Vicat Softening Point 160 °C320 °FRate B/50; ASTM D1525
 161 °C322 °FRate B/50; ISO 306
 162 °C324 °FRate B/120; ISO 306
UL RTI, Electrical 105 °C221 °FUL 746B
UL RTI, Mechanical with Impact 105 °C221 °FUL 746B
UL RTI, Mechanical without Impact 105 °C221 °FUL 746B
Flammability, UL94  V-0
@Thickness >=1.50 mm
V-0
@Thickness >=0.0591 in
UL 94
 5VA
@Thickness >=2.00 mm
5VA
@Thickness >=0.0787 in
UL 94
Glow Wire Ignition Temperature  800 °C
@Thickness 3.00 mm
1470 °F
@Thickness 0.118 in
IEC 60695-2-13
 825 °C
@Thickness 1.00 mm
1520 °F
@Thickness 0.0394 in
IEC 60695-2-13
 825 °C
@Thickness 1.50 mm
1520 °F
@Thickness 0.0591 in
IEC 60695-2-13
 825 °C
@Thickness 2.00 mm
1520 °F
@Thickness 0.0787 in
IEC 60695-2-13
Glow Wire Flammability Index  960 °C
@Thickness 1.50 mm
1760 °F
@Thickness 0.0591 in
IEC 60695-2-12
 960 °C
@Thickness 2.00 mm
1760 °F
@Thickness 0.0787 in
IEC 60695-2-12
 960 °C
@Thickness 3.00 mm
1760 °F
@Thickness 0.118 in
IEC 60695-2-12
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 300 - 325 °C572 - 617 °F
Zone 2 275 - 320 °C527 - 608 °F
Zone 3 290 - 325 °C554 - 617 °F
Melt Temperature 300 - 325 °C572 - 617 °FInjection Molding
Mold Temperature 80.0 - 110 °C176 - 230 °F
Drying Temperature 110 - 120 °C230 - 248 °FInjection Molding
Dry Time 3.00 - 4.00 hour3.00 - 4.00 hourInjection Molding
 8.00 hour8.00 hourCumulative; Injection Molding
Back Pressure 0.300 - 0.700 MPa43.5 - 102 psi
Shot Size 30 - 70 %30 - 70 %
Screw Speed 20 - 100 rpm20 - 100 rpm
 
Descriptive Properties
UV-light, water exposure/immersionF1UL 746C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH82397 / 290344

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.