Hostacom G2 U02 102297 is a 20% glass fiber reinforced PP homopolymer, with high flowability, high stiffness and low creep under load at elevated temperatures. This grade is delivered in black 102297 color version. Applications: UnderhoodInformation provided by LyondellBasell. |