MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Trinseo INSPIRE™ DLGF 9631.01 Z Polypropylene homopolymer, 60% LGF  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Overview: DLGF 9631.01 Z is based on polypropylene homopolymer and reinforced with 60% by weight of long glass fiber. (PP-LGF 60, Long Glassfiber Granulate). DLGF 9631.01 Z is produced by pultrusion/meltipregnation process, therby ensuring through impregnation of all the filaments in the glassfiber-roving and also providing improve ‘pellet robustness’ for air conveying. It is available in ‘standard black’ color (TR 7701862). This PP-LGF60 is a ‘concentrate’ which has to be diluted – usually with ‘neat’-PP but also mineral-filled PP-based compounds can be used. The ‘dilution’ is typically done as a dry-blend of granulates by means of gravimetric dosing devices at the injection-molding machine. A weight ratio of 1 : 1 of DLGF 9631.01 Z and i.e. LGF 8100 PP-copolymer will result in a composite-material-system have 30% by weight of glassfiber. The ‘long’ glass fiber (initial length = 11 mm) provide high stiffness, strength and impact-resistance to the injection molded parts. DLGF 9631.01 Z has been especially formulated to meet the requirements for use in automotive ‘under-the-hood’ (UTH) and ‘under-body’ applications i.e. front-end carriers (FEC) aka ‘bolster’, impingement shields or structural parts like i.e. battery trays or spare wheel wells. The long term heat ageing resistance (LTHA) has been increased to a high level of needed for ‘UTH” applications. Injection molded parts based on DLGF 9631.01 Z diluted with ‘neat’-PP to 30% GF-content will show no signs of degradation and surpass the limit of >100 h @ 150°C. When diluted to 40% GF-content, the heat aging performance of compsites based on DLGF 9631.01 Z will increase beyond the 1000 h. In many cases, even a dilution to 20% will result passing beyond 1000 h @ 150°C, however this will depend on the wall-thickness of moded parts as well as the choice of dilution resin and therefore, it is recommended to conduct own tests.

Information provided by Styron

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.12 g/cc0.0405 lb/in³ISO 1183
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 105 MPa15200 psiISO 527-2/50
Elongation at Break 2.3 %2.3 %ISO 527-2/50
Tensile Modulus 6.50 GPa943 ksiISO 527-2/5
Flexural Strength 155 MPa22500 psi3-Point Bending; ISO 178
Flexural Modulus 6.50 GPa943 ksi3-Point Bending; ISO 178
Izod Impact, Notched 2.30 J/cm
@Temperature 23.0 °C
4.31 ft-lb/in
@Temperature 73.4 °F
ASTM D256
Izod Impact, Unnotched (ISO) 17.0 kJ/m²
@Temperature 23.0 °C
8.09 ft-lb/in²
@Temperature 73.4 °F
ISO 180
Charpy Impact Unnotched  4.50 J/cm²
@Temperature 23.0 °C
21.4 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1fU
 5.30 J/cm²
@Temperature 23.0 °C
25.2 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
Multi-axial Impact @ -30°C Total Energy 19.0 J
@Thickness 4.00 mm,
Temperature 23.0 °C
14.0 ft-lb
@Thickness 0.157 in,
Temperature 73.4 °F
4.4 m/sec, 20 mm Striker Diameter; Support = 40 mm; ISO 6603-2
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 155 °C311 °FASTM D648; ISO 75-2/A

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Trinseo INSPIRE™ DLGF 9621.00 Compounded Polypropylene, 60% LGF
Buckeye Polymers BP RPP 0511C Polypropylene, 5% Mineral Filled
Multibase Multi-Pro® 1012 C BLK Medium Impact Mineral Filled Polypropylene
Trinseo LGF 9621 Homopolymer Polypropylene
Buckeye Polymers BP RPP 1012 C Polypropylene, 10% Mineral Filled

PZZDWST065 / 142274

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.