MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Solvay LTM® 45 Epoxy Prepreg
Categories: Polymer; Thermoset; Epoxy

Material Notes: Description: LTM45 series pregregs consists of a range of low temperature curing epoxy matrix resins giving pregpregs with elevated end use temperature performance and good hot and wet strength retention. The range encompases LTM45 with an initial cure temperature of 50°C (122°F). All the resins within the range exhibit similar thermo-mechanical performance when fully cured. LTM45 and LTM45-EL are the most commonly selected prepreg resin systems from this range. For improved oven vacuum processing LTM45-1 is recommended as an alternative to LTM45EL when used with carbon fabrics up to 285 g/m2. LTM45-1 provides improved toughness and compression properties.

Features & Benefits:

  • Low initial cure temperature at 50°C (122°F)
  • Rapid cure at conventional temperatures
  • 180°C (356°F) Tg after suitable post-cure
  • May be processed by vacuum bag or autoclave (also see data sheet PDS1082 covering LTMS45-1 in detail)
  • Available with a wide range of woven and unidirectional reinforcements including carbon, glass, aramid specialist fibers and hybrids
  • 180°C (356°F) service parts molded direct from low cost masters
  • Good mechanical properties
Product Variants: LTM45B- Black pigmented version of LTM45

Information provided by Cytec, subsequently acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.20 g/cc2 hrs at 120°C
Storage Temperature -18.0 °C
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 180 °C
Glass Transition Temp, Tg 65.0 °CDMA E' onset, 24 hrs at 50°C
 180 °CDMA E' onset, 24 hrs at 50°C+2 hrs at 180°C
 
Processing PropertiesOriginal ValueComments
Shelf Life 6.00 Month

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Solvay LTM® 45EL Epoxy Prepreg
Armacell Ensolite™ MLC-Black PVC/NBR
Chlorosulfonated Polyethylene Rubber (CM, CSM)
Polynorbornene Rubber (PNR)
Solvay CYCOM® 977-6 Epoxy Laminate with IM7 Unidirectional Tape

PCYTED141 / 180443

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.