MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Morgan Advanced Ceramics IFB Structural Insalcor® Thermal Ceramic
Categories: Ceramic; Oxide

Material Notes: Manufacturing method: extrusion. These products offer superior performance in load bearing applications and in conditions where abrasion from mechanical and chemical abuse or flow of hot gases is severe. Our Structural Range of IFB deliver big energy savings for many markets and our global manufacturing footprint enables Morgan to meet your regional and global application demands.

Applications: Hot face refractory lining or as back-up insulation in:

  • Petrochemical (kilns, flues, refining vessels and heaters and reactor chambers)
  • Iron and steel industry (heat treatment and galvanising)
  • Coke and iron making (blast furnaces, hot blast stoves, hot blast and bustle main)
  • Ceramic industry (including kilns for domestic use)
  • Glass industry
  • Power generation

Information provided by Morgan Advanced Materials

Key Words: Thermal Ceramics
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.314 g/cc0.04747 lb/in³ASTM C-133
Deformation 0.10 %
@Temperature 1450 °C,
Time 5400 sec
0.10 %
@Temperature 2640 °F,
Time 1.50 hour
0.069 MPa; ASTM C-16
 
Mechanical PropertiesMetricEnglishComments
Modulus of Rupture 0.00240 GPa0.348 ksiASTM C-133
Compressive Strength 6.90 MPa1000 psiCold Crushing Strength; ASTM C-133
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity  0.790 W/m-K
@Temperature 260 °C
5.48 BTU-in/hr-ft²-°F
@Temperature 500 °F
ASTM C-182
 0.800 W/m-K
@Temperature 540 °C
5.55 BTU-in/hr-ft²-°F
@Temperature 1000 °F
ASTM C-182
 0.910 W/m-K
@Temperature 815 °C
6.32 BTU-in/hr-ft²-°F
@Temperature 1500 °F
ASTM C-182
 1.09 W/m-K
@Temperature 1100 °C
7.56 BTU-in/hr-ft²-°F
@Temperature 2010 °F
ASTM C-182
 1.33 W/m-K
@Temperature 1370 °C
9.23 BTU-in/hr-ft²-°F
@Temperature 2500 °F
ASTM C-182
Shrinkage 0.40 %
@Treatment Temp. 1730 °C,
Time 86400 sec
0.40 %
@Treatment Temp. 3150 °F,
Time 24.0 hour
ASTM C-210
 
Component Elements PropertiesMetricEnglishComments
Al2O3 77 %77 %
CaO 0.10 %0.10 %
Fe2O3 0.40 %0.40 %
Other 0.40 %0.40 %MgO + Na2O + K2O
SiO2 21 %21 %
TiO2 0.60 %0.60 %
 
Descriptive Properties
Classification Temperature (°C)1790
Reversible Linear Expansion (%)1.2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

CMORF6209 / 202993

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.