MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

n-Butyric acid (Butanoic acid), C4H8O2
Categories: Fluid; Solvent

Key Words: C4H8O2
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.958 g/cc
@Temperature 20.0 °C
0.0346 lb/in³
@Temperature 68.0 °F
Viscosity 1.55 cP
@Temperature 20.0 °C
1.55 cP
@Temperature 68.0 °F
Dynamic Viscosity
Molecular Weight 88.107 g/mol88.107 g/mol
Vapor Pressure 0.000708 bar
@Temperature 20.0 °C
0.531 torr
@Temperature 68.0 °F
Surface Tension 26.8 dynes/cm
@Temperature 20.0 °C
26.8 dynes/cm
@Temperature 68.0 °F
 
Chemical PropertiesMetricEnglishComments
Critical Pressure 52.7 bar39500 torr
Critical Temperature 355 °C671 °F
Critical Density 0.302 g/cc0.0109 lb/in³
Critical Molar Volume 292 cm³/mol17.8 in³/mol
 
Thermal PropertiesMetricEnglishComments
Heat of Vaporization 476.8 J/g205.1 BTU/lb
Specific Heat Capacity 1.304 J/g-°C
@Temperature 25.0 °C
0.3117 BTU/lb-°F
@Temperature 77.0 °F
Vapor
Thermal Conductivity 0.1481 W/m-K
@Temperature 20.0 °C
1.028 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
Melting Point -5.30 °C22.5 °F
Boiling Point 163.3 °C325.9 °F
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.396
@Wavelength 589.3 nm
1.396
@Wavelength 589.3 nm
nD
 
Descriptive Properties
Antoine's Vapor Pressure A Parameter17.924
Antoine's Vapor Pressure B Parameter4130.93
Antoine's Vapor Pressure C Parameter-70.55
Antoine's Vapor Pressure Formulaln πp = A - B/(T+C)P in mmHg and T in K
CAS registry number (CARN)107-92-3
Chemical FormulaC4H8O2
Critical Compressibility (Zc)0.295
Dipole moment (p/C.m)5.003E-28
Dynamic Viscosity Formulalog10 η=A(1/T-1/B)
Dynamic Viscosity Parameter A640.42
Dynamic Viscosity Parameter B321.13
Molar Heat Capacity (298K)114.871 J/mol-K
Molar Heat Capacity of Vapor a Parameter11.7319
Molar Heat Capacity of Vapor b Parameter0.4134
Molar Heat Capacity of Vapor c Parameter-0.0002428
Molar Heat Capacity of Vapor d Parameter5.527E-08
Molar Heat Capacity of Vapor FormulaCp = a + bT + cT2 + dT3Cp in J/mol-K
UN Number2820

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

VORGS057 / 99445

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.