Special, pure white compound with excellent high temperature properties and wide chemical resistance. Extremely low outgassing properties. Applications: For use in applications which require exposure to temperatures in excess of 260°C (500°F) and shorter term to 310°C (590°F). Recommended for use in the semiconductor industry. Do not use any Perlast ® grade with molten alkali metals. |