MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Solvay MIRACARE® SLB-365/N Surfactant  (discontinued **)
Categories: Fluid

Material Notes: Description: Surfactant blend used in the production of structured liquid formulations. The preservative in MIRACARE SLB-365/N is a non-formaldehyde donor (Neolone).

I.N.C.I. Name: WATER, SODIUM TRIDECETH SULFATE, SODIUM LAUROAMPHOACETATE, COCAMIDE MEA, SODIUM CHLORIDE, METHYLISOTHIAZOLINONE

CAS: 7732-18-5, 25446-78-0, 68608-66-2, 68140-00-1, 7647-14-5, 2682-20-4

EINECS / ELINCS: 231-791-2, 246-985-2, 271-794-6, 268-770-2, 231-598-3, 220-239-6

Available in: Asia Pacific, Europe, Latin America and North America

Applications: MIRACARE SLB-365/N is a completely formulated free flowing high active Performance Concentrate used in the preparation of structured liquids formulations. When used as prescribed MIRACARE SLB-365/N will yield spherulitic formulations capable of suspending & delivering oils and actives in various skin cleanser formulations. Typical applications are body washes, skin cleansers, facial cleansers, and shampoos.

Information provided by Rhodia, Rhodia has been acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.10 g/cc0.0397 lb/in³
Solids Content 48 - 52 %48 - 52 %Microwave; RP-17650
pH 9.0 - 109.0 - 1010% Solution; RP-17601
Viscosity 1000 - 5000 cP1000 - 5000 cP#3 Spindle, 12 rpm >1 min; RP-17619
 
Optical PropertiesMetricEnglishComments
Gardner Color Number <= 2.0<= 2.025% in DI; RP-17602
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month12.0 Month
 
Descriptive Properties
AppearanceHazy, pourable liquidRP-0064
CompositionActive37-42%, MW 434, RP-17501
 Methylisothiazolinone0.0035-0.0045%
 Microbial Count<1.0 cfu/ml, RP-1370
 Sodium Chloride<2.5%, RP-17504
 Sodium Sulfate<0.6%, RP-17503
Foreign MatterFree from foreign matter

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Solvay MIRACARE® SLB-365/G Surfactant
Solvay MIRACARE® SLB-205/N Surfactant

WRHOD249 / 137480

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.