MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Dow Silastic® 9206-30 LSR Oil-Bleeding Liquid Silicone Rubber  (discontinued **)
Categories: Polymer; Thermoset; Silicone; Silicone Rubber; Liquid Silicone Rubber (LSR)

Material Notes: Standard grade, oil-filled, self-lubricating LSR. SILASTIC™ 920x-yy Series LSRs where x = oil content and yy = Durometer hardness.

Product applications:

  • Automotive connector seals
  • Electrical connections
  • Weatherpack seals
Key Features:
  • Oil filled
  • Low compression set
  • Low viscosity
  • Unique rheology
  • Opaque

Former Dow/ Dow Corning brand.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.11 g/cc1.11 g/ccASTM D792
Viscosity  160000 cP
@Frequency 10 Hz
160000 cP
@Frequency 10 Hz
Part B; CTM 1094
 190000 cP
@Frequency 10 Hz
190000 cP
@Frequency 10 Hz
Part A; CTM 1094
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 3030ASTM D2240
Tensile Strength 5.50 MPa798 psiASTM D412
Elongation at Break 530 %530 %ASTM D412
Tear Strength 39.0 kN/m223 pliASTM D624 DIE B
Compression Set 18 %
@Temperature 175 °C,
Time 79200 sec
18 %
@Temperature 347 °F,
Time 22.0 hour
NPC; ASTM D395
 
Descriptive Properties
Oil Content. Weight %6

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Rogers Corporation Bisco™ HT-6000 Solid Silicone Rubber
Precision Polymer Engineering S50R Silicone Rubber
NuSil LSR-5850 Liquid Silicone Rubbers (LSR)
Momentive Performance Materials Addisil™ 1070 E Industrial Extrusion Heat Cured Rubber
LG Chemical 1.3-Butadiene

PDOW9927 / 233130

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.