MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Lubrizol Advanced Materials Pearlbond® DIPP-119 Thermoplastic Polyurethane
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Pearlbond™ DIPP-119 is polycaprolactone copolyester based thermoplastic polyurethane, supplied in form of translucent pellets. Featuring low melting point and excellent transparency, this product offers excellent flexibility, elasticity and easy processing. Ideally used for extrusion or compound with PVC.

Applications: Pearlbond™ DIPP-119 is used mostly in extrusion applications where low melting point as well as improved adhesion over polar substrates is highly appreciated. It is ideal for PVC compounding. It is also used in solvent coating on textile substrates.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.16 g/cc1.16 g/ccISO 2781
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7070ISO 2781
Tensile Strength at Break 20.0 MPa2900 psiISO 527-2/5A/500
Tensile Stress at Strain  3.00 MPa
@Strain 100 %
435 psi
@Strain 100 %
ISO 527-2/5A/500
 4.00 MPa
@Strain 300 %
580 psi
@Strain 300 %
ISO 527-2/5A/500
Elongation, Ultimate 750 %750 %ISO 527-2/5A/500
Tear Strength 50.0 kN/m285 pli[mm3]; ISO 34-1B
Abrasion 4545ISO 4649-A
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 40.0 °C104 °FISO 306 (A50)
 
Processing PropertiesMetricEnglishComments
Zone 1 125 °C257 °F
Zone 2 150 °C302 °F
Zone 3 165 °C329 °F
Zone 4 170 °C338 °F
Adapter Temperature 170 °C338 °F(5)
Die Temperature 150 °C302 °F(6)
 150 °C302 °FTIP (7)
Drying Temperature 70.0 °C158 °F
Dry Time 3.00 - 4.00 hour3.00 - 4.00 hour
Dew Point -40.0 °C-40.0 °F
 
Descriptive Properties
AppearanceTranslucent
Taber Loss45 mm3DIN 53,516

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMEQU955b / 179136

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.