MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Phillips 66 Kendall® GT-1® Motor Oil with Liquid Titanium®, SAE Grade 30
Categories: Fluid; Lubricant

Material Notes: Kendall® GT-1® Motor Oil with Liquid Titanium® protection additive is a high quality, conventional automotive engine oil designed for use in gasoline-fueled passenger cars and light trucks that do not require an ILSAC GF-5 oil for warranty coverage. GT-1 Motor Oil with Liquid Titanium is formulated to provide excellent wear protection, to minimize sludge and varnish formation, and to resist viscosity and thermal breakdown, even in severe service. It also protects against rust and bearing corrosion, and is highly resistant to foaming. All viscosity grades are fortified with our exclusive Liquid Titanium protection additive for extra protection against engine wear. This additive enhancement provides increased engine protection by forming a strongly bonded titanium shield on the surface of critical engine parts, which reduces friction and wear and can help extend engine life.

Applications:

  • Gasoline-fueled passenger cars, light trucks and sport utility vehicles that do not require an ILSAC GF-5 oil for warranty coverage
  • Older vehicles where the engine manufacturer specifies monograde engine oil
GT-1 Motor Oil with Liquid Titanium is licensed:
  • API Service SN
Features/Benefits:
  • Exclusive Liquid Titanium protection additive provides extra protection against engine wear
  • Excellent resistance to viscosity and thermal breakdown at high temperatures
  • Protects against sludge and varnish formation
  • Protects against rust and bearing corrosion
  • Highly resistant to foaming

Information provided by Phillips 66 Lubricants.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.882 g/cc
Density 7.35 lb/gal
Viscosity 3.4 cP
@Temperature 150 °C
High-Temp/High-Shear
Viscosity Measurement 109Index
Kinematic Viscosity at 40°C (104°F) 95 cSt
Kinematic Viscosity at 100°C (212°F) 11.5 cSt
Ash 1.1 %Sulfated; ASTM D874
ASTM Color 3.5ASTM D1500
 
Chemical PropertiesOriginal ValueComments
Total Base Number 9.3ASTM D2896
 
Thermal PropertiesOriginal ValueComments
Pour Point -33.0 °C
Flash Point 250 °CCOC
 
Component Elements PropertiesOriginal ValueComments
Phosphorus, P 0.089 %
Titanium, Ti 0.010 %
Zinc, Zn 0.098 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WCON5383 / 198636

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.