MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
RTP Company RTP 304 FR Polycarbonate (PC), Glass Fiber - Flame Retardant - Non-PBBO/E - UL94 V-0
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Glass Fiber Filled, Flame Retardant

Material Notes: The RTP series of flame retardant, glass fiber reinforced polycarbonate materials offer dimensional stability with improved heat distortion and ignition resistance performance over the base resin.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.38 g/ccASTM D 792
Filler Content 25 %Primary Additive
Water Absorption 0.080 %24 hrs @ 23°C; ASTM D 570
Linear Mold Shrinkage 0.0015 - 0.0030 cm/cm
@Thickness 3.17 mm
ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 118ASTM D 785
Tensile Strength at Break 16000 psiASTM D 638
Elongation at Break 3.0 - 4.0 %ASTM D 638
Tensile Modulus 1050 ksiASTM D 638
Flexural Strength 25000 psiASTM D 790
Flexural Modulus 950 ksiASTM D 790
Izod Impact, Notched 2.80 ft-lb/in
@Thickness 3.17 mm
D 256
Izod Impact, Unnotched 14.0 ft-lb/in
@Thickness 3.17 mm
ASTM D4812
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+16 ohm-cmASTM D 257
Dielectric Constant 3.3
@Frequency 1e+6 Hz
Dry; ASTM D 150
Dielectric Strength 470 V/milShort Term; in oil; ASTM D 149
Dissipation Factor 0.0080
@Frequency 1e+6 Hz
Dry; ASTM D 150
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 295 °FASTM D 648
Deflection Temperature at 1.8 MPa (264 psi) 290 °FASTM D 648
Flammability, UL94 V-0
@Thickness 1.59 mm
 
Processing PropertiesOriginal ValueComments
Melt Temperature 550 - 600 °F
Mold Temperature 180 - 250 °F
Drying Temperature 250 °F
Dry Time 4 hour
Moisture Content 0.020 %
Dew Point -20.0 °F
Injection Pressure 10000 - 15000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Covestro Bayblend® FR3010 HF PC/ABS Blend
RTP Company RTP 300 TFE 20 SE Polycarbonate (PC), Unreinforced - PTFE Lubricated - Self Extinguishing - Bromine/Chlorine Free - UL94 V-0
Covestro Makrolon® 6487 Polycarbonate, Flame Retardant Grade
Covestro Bayblend® FR3006 HF PC/ABS Blend
Covestro Bayblend® ET3032 FR Rubber Modified PC Blend, 10% Mineral Filled

PQZWA1154 / 90623

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.