MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

NOVA Chemicals NOVAPOL® PF-0218-F LLDPE Film Resin
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade

Material Notes:

Butene Copolymer

Features:

  • Toughness and strength
  • Ease of extrusion

Additives:

  • Processing Antioxidant

Applications:

  • Stretch wrap
  • Blend resin
  • Industrial packaging

Film properties are typical of blown film extruded on a 2.5" extruder with 4" die and 100-mil die gap at a blow up ratio of 2.5:1, but are dependent upon operating conditions.

United States: NOVAPOL PF-0218 Series resin complies with the specifications contained in the U.S. Food and Drug Administration (FDA) regulation 21 CFR 177.1520 for olefin polymers, para. (c) 3.2a, and may thus be used in the United States as an article or component of an article intended for use in contact with food, without temperature or food-type restrictions, subject to technical suitability.

NOVA Chemicals polyethylene resins are biologically and chemically inert.

Information provided by NOVA Chemicals®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.918 g/cc0.0332 lb/in³ASTM D 792
Thickness 25.0 microns0.984 mil
Melt Index of Compound 2.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
2.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D 1238
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 10.0 MPa1450 psiASTM D 882
Film Tensile Strength at Yield, TD 10.0 MPa1450 psiASTM D 882
Film Elongation at Break, MD 660 %660 %ASTM D 882
Film Elongation at Break, TD 700 %700 %ASTM D 882
Elmendorf Tear Strength MD 110 g110 gASTM D 1922
Elmendorf Tear Strength TD 330 g330 gASTM D 1922
Dart Drop Test 100 g0.221 lbF50; ASTM D 1709/A
Film Tensile Strength at Break, MD 32.0 MPa4640 psiASTM D 882
Film Tensile Strength at Break, TD 25.0 MPa3630 psiASTM D 882
1% Secant Modulus, MD 170 MPa24700 psiASTM D 882
1% Secant Modulus, TD 190 MPa27600 psiASTM D 882
 
Optical PropertiesMetricEnglishComments
Haze 14 %14 %ASTM D 1003
Gloss 43 %43 %@ 45°; ASTM D 2457
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.
 
Descriptive Properties
Low Friction Puncture (J/mm)29NOVA Chemicals test method

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
NOVA Chemicals Novapol® PF-0218-B Butene Copolymer LLDPE Film Resin
NOVA Chemicals Novapol® PF-0218-E Butene Copolymer LLDPE Film Resin
NOVA Chemicals NOVAPOL® PF-0218-B LLDPE Film Resin

PNOVB031 / 194639

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.