MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Toyobo Celanex® XFR 6842 GF30 HRHP PBT, Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant

Material Notes: Product Description: Celanex XFR 6842 GF30 HRHP is a halogen and antimony free flame retardant (V-0 @ 0.8 mm) glass reinforced PBT grade with good processability and excellent hydrolysis resistance. It is suitable for parts requiring enhanced tracking resistance, toughness and flame retardancy. The product is WEEE and RoHS compliant.

Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America

Filler/Reinforcement: Glass Fiber

Additive: Flame Retardant; Hydrolysis Resistant

Features: Flame Retardant; Hydrolysis Resistant

Forms: Pellets

Processing Method: Injection Molding

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Water Absorption 0.20 %0.20 %Equilibrium, 50% RH; ISO 62
Melt Flow 7.0 g/10 min
@Load 5.00 kg,
Temperature 250 °C
7.0 g/10 min
@Load 11.0 lb,
Temperature 482 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 115 MPa16700 psiISO 527-2/50
Elongation at Break 2.2 %2.2 %ISO 527-2/5
Tensile Modulus 10.0 GPa1450 ksiISO 527-1
Charpy Impact Unnotched 4.62 J/cm²22.0 ft-lb/in²ISO 179/1eU
Charpy Impact, Notched 0.798 J/cm²3.80 ft-lb/in²ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Comparative Tracking Index 475 V475 V50 drops; IEC 60112
 
Thermal PropertiesMetricEnglishComments
Melting Point 225 °C437 °FISO 11357-3
Flammability, UL94  V-0
@Thickness 0.787 mm
V-0
@Thickness 0.0310 in
 V-0
@Thickness 1.52 mm
V-0
@Thickness 0.0600 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHCQ6213 / 310906

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.