MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Bohler-Uddeholm moldMAX® XL High Strength Copper Alloy  (discontinued **)
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: moldMAX® XL is characterized by:
  • High thermal conductivity
  • Excellent machinability
  • Good polishability and
  • Good corrosion resistance
  • Good wear resistance
  • High impact strength
  • Excellent resistance to galling
  • Large cross sectional availability

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.322 lb/in³hardened to 30 HRC
 0.316 lb/in³
@Temperature 299 °C
hardened to 30 HRC
 0.317 lb/in³
@Temperature 199 °C
hardened to 30 HRC
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell C 28 - 32Delivery condition
Tensile Strength, Ultimate 110000 psihardened to 30 HRC
Tensile Strength, Yield 100000 psi
@Strain 0.2 %
hardened to 30 HRC
Elongation at Break 5.0 %hardened to 30 HRC
Modulus of Elasticity 17000 ksi(hardened to 30 HRC)
Compressive Yield Strength 655 MPa0.2%, hardened to 30 HRC
 
Thermal PropertiesOriginal ValueComments
CTE, linear 9.50 µin/in-°F
@Temperature 199 °C
hardened to 30 HRC
 9.70 µin/in-°F
@Temperature 299 °C
hardened to 30 HRC
Specific Heat Capacity 0.0910 BTU/lb-°F
@Temperature 20.0 °C
hardened to 30 HRC
 0.0970 BTU/lb-°F
@Temperature 199 °C
hardened to 30 HRC
 0.103 BTU/lb-°F
@Temperature 299 °C
hardened to 30 HRC
Thermal Conductivity 61.0 W/m-K
@Temperature 20.0 °C
hardened to 30 HRC
 92.0 W/m-K
@Temperature 199 °C
hardened to 30 HRC
 105 W/m-K
@Temperature 299 °C
hardened to 30 HRC
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu 85 %
Nickel, Ni 9.0 %
Tin, Sn 6.0 %

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ampco Metal AMPCOLOY® 940 Nickel-Copper, Extrusion, 25 - 50 mm.
Schmolz + Bickenbach MoldMAX® V Copper Alloy
Ampco Metal AMPCOLOY® 83 Beryllium Copper, Extrusion
Total PPH 3620WZ Polypropylene, Injection Molding Grade
A. Schulman ComAlloy Lubrilon® 604 Nylon 6/6, PTFE/Molybdenum Disulfide Filled, Flow Enhanced

NBUCOR31 / 15500

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.