MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Shin-Etsu Silicones SV-14000U Silicone Rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Silicone; Silicone Rubber

Material Notes: SV14000U is one of a series of easy processing, no post cure silicone rubber bases. It can be used in a variety of applications requiring finishing by molding, extruding or calendering.

Product Features:

  • This product can be blended with other ShinEtsu general purpose or no post cure bases for intermediate properties. The choice between these bases will depend on specific requirements. This product can also be extended with filler.
Typical Applications:
  • Roll covers.
  • Diaphragms.

Information Provided by Shin-Etsu Silicones of America, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.09 g/cc1.09 g/ccDCBP Cure
 1.09 g/cc1.09 g/ccDBPH Cure
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 4040DCBP Cure
 4141DBPH Cure
Tensile Strength at Break 5.12 MPa742 psiDCBP Cure
 6.55 MPa950 psiDBPH Cure
Elongation at Break 360 %360 %DCBP Cure
 437 %437 %DBPH Cure
100% Modulus  0.972 MPa
@Strain 100 %
141 psi
@Strain 100 %
DBPH Cure
 1.06 MPa
@Strain 100 %
154 psi
@Strain 100 %
DCBP Cure
Tear Strength 10.7 kN/m61.0 pliDie B; DCBP Cure
 11.6 kN/m66.0 pliDie B; DBPH Cure
Compression Set 25 %
@Temperature 177 °C,
Time 79200 sec
25 %
@Temperature 351 °F,
Time 22.0 hour
DCBP Cure
 
Processing PropertiesMetricEnglishComments
Cure Time 10.0 min0.167 hour
 
Descriptive Properties
Cure AgentDBPH
 DCBP
Cure TypePress Cure

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Shin-Etsu Silicones KE-1052A/B Silicone, Gel RTV
Shin-Etsu Silicones LIMS™ KE1950-70A/B Elastomer
Shin-Etsu Silicones SV-18000U Silicone Rubber
Shin-Etsu Silicones SV-58000U High Strength Silicone Elastomer
Shin-Etsu Silicones FE-371U Fluorosilicone Elastomer

PSHIN256 / 177767

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.