MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Prodways PRINT3D Hydroxyapatite Powder for 3D Printing
Categories: Ceramic

Material Notes: PRINT3D Hydroxyapatite is a ceramic resin used for biomedical applications. Combined with the Prodways ProMaker V6000 ceramic 3D printer, it allows for the production of biocompatible, non-resorbable parts with a chemical structure close to that of bone, with a very high level of detail, like implants, prosthesis and bone substitutes for reconstructive surgery.

Information provided by Prodways

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Porosity 7.0 %Finished Product
 
Mechanical PropertiesOriginal ValueComments
Vickers Microhardness 0.455GPa
Compressive Strength 170 MPa

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Calcium Hydroxyapatite, Ca10(PO4)6(OH)2
Zeus AbsorvĀ® Poly(e-caprolactone) (PCL) Bioabsorbable Polymer
Beijing Evergrow Resources Carbon Fiber Tissue
Americas Styrenics EA6740 High Impact Polystyrene
Rogers Arlon 25188T017 Silicone Rubber/Laminated ETFE Film

PPRODW965 / 220983

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.