MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Avient FireCon™ CPE 30-2 Natural Chlorinated Polyethylene (CPE)  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: An excellent choice for low-voltage power-and-cable control cables, this filled, flexible thermoplastic CPE jacketing compound offers wire and cable manufacturers the advantages of thermoplastic extrusion processing without the need to invest in continuous vulcanization (CV) equipment. CPE 30-2 Natural allows manufacturers to color jacketing products. This grade has application for fiber optic cable that is used in harsh environments requiring high-performance jacketing that is chemical and oil resistant, flame retardant. This grade is colorable, without compromising these performance requirements. CPE 30-2 NAT can be processed in a wide range of colors with PolyOne's color products.

Pre-drying is recommended for 4 hours at 175°-185°F. Typical processing temperatures range between 320°-390°F depending upon screw design. Typical Properties of Molded Slab (0.075"); Not to be Construed as Specifications.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.28 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 47
@Time 10.0 sec
ASTM D2240
Tensile Strength at Break 11.0 MPaType IV, 510 mm/min; ASTM D638
Elongation at Break 420 %Type IV, 510 mm/min; ASTM D638
Tensile Modulus 6.89 MPaType IV, 510 mm/min; ASTM D638
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature -18.0 °CASTM D746
Oxygen Index 29 %
@Thickness 1.91 mm
ASTM D2863
 
Descriptive Properties
AppearancePellets/CubesASTM D2090
FeaturesFlame Retardant
 Good Chemical Resistance
 Oil Resistant
FormsPellets
Generic NamePolyethylene, Chlorinated (CPE)
Regional AvailabilityAsia Pacific
 North America
 South America
Retention of Elongation, %80168 hr, UL Standard; 121°C, 1.91 mm
Retention of Tensile Strength, %110168 hr, UL Standard; 121°C, 1.91 mm
UsesCable Jacketing
 Fiber Optic Cable
 Wire & Cable Applications

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Avient FireCon™ CPE 30-2 RoHS BLACK Polyethylene, Chlorinated (CPE)
Avient FireCon™ CPE-37-11 RoHS Black Polyethylene, Chlorinated (CPE)
Avient PolyOne® CPE 30-2 Chlorinated Polyethylene (CPE)
BorsodChem ONGRO CPE 3602 N Chlorinated Polyethylene
BorsodChem ONGRO CPE 3602 C Chlorinated Polyethylene

PH1PN8139 / 101975

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.