MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lord Adhesives Thermoset™ MD-130 Electrically Insulating Die-Attach Adhesive
Categories: Polymer; Adhesive

Material Notes: Lord MD-130 is a microelectronic grade, die-attach adhesive system for use in applications where electrical conductivity is not required. This system offers long, room temperature stability, fast cure at temperatures down to 100°C, and high die-shear strengths.

All information provided by Lord.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.49 g/cc
@Temperature 25.0 °C
1.49 g/cc
@Temperature 77.0 °F
Water Absorption 0.050 %0.050 %
Viscosity 60000 cP60000 cP
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8888
Tensile Strength, Yield 56.5 MPa8200 psi
Elongation at Yield 1.7 %1.7 %
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmASTM D257
Dielectric Constant 4.2
@Frequency 1000 Hz,
Temperature 25.0 °C
4.2
@Frequency 1000 Hz,
Temperature 77.0 °F
ASTM D150
Dissipation Factor 0.0080
@Frequency 1000 Hz,
Temperature 25.0 °C
0.0080
@Frequency 1000 Hz,
Temperature 77.0 °F
ASTM D150
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.418 W/m-K2.90 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 130 °C266 °F
Minimum Service Temperature, Air -55.0 °C-67.0 °F
Glass Transition Temp, Tg 140 °C284 °FMettler DSC30
 
Processing PropertiesMetricEnglishComments
Cure Time  4.00 min
@Temperature 150 °C
0.0667 hour
@Temperature 302 °F
Hot Plate
 8.00 min
@Temperature 150 °C
0.133 hour
@Temperature 302 °F
Oven
 16.0 min
@Temperature 135 °C
0.267 hour
@Temperature 275 °F
Oven
 20.0 min
@Temperature 135 °C
0.333 hour
@Temperature 275 °F
Hot Plate
 34.0 min
@Temperature 120 °C
0.567 hour
@Temperature 248 °F
Hot Plate
 48.0 min
@Temperature 120 °C
0.800 hour
@Temperature 248 °F
Oven
 68.0 min
@Temperature 100 °C
1.13 hour
@Temperature 212 °F
Hot Plate
 148 min
@Temperature 100 °C
2.47 hour
@Temperature 212 °F
Oven
Gel Time  1.00 min
@Temperature 150 °C
1.00 min
@Temperature 302 °F
Hot Plate
 2.00 min
@Temperature 150 °C
2.00 min
@Temperature 302 °F
Oven
 4.00 min
@Temperature 135 °C
4.00 min
@Temperature 275 °F
Oven
 5.00 min
@Temperature 135 °C
5.00 min
@Temperature 275 °F
Hot Plate
 8.00 min
@Temperature 120 °C
8.00 min
@Temperature 248 °F
Hot Plate
 12.0 min
@Temperature 120 °C
12.0 min
@Temperature 248 °F
Oven
 17.0 min
@Temperature 100 °C
17.0 min
@Temperature 212 °F
Hot Plate
 37.0 min
@Temperature 100 °C
37.0 min
@Temperature 212 °F
Oven
Shelf Life  6.00 Month
@Temperature 25.0 °C
6.00 Month
@Temperature 77.0 °F
 12.0 Month
@Temperature 4.00 °C
12.0 Month
@Temperature 39.2 °F
 
Descriptive Properties
AppearanceBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Epoxy Adhesive
Tra-Con Tra-Cast 3107 Low Shrinkage Epoxy Casting System
Tra-Con Tra-Cast 3104 Low Viscosity Epoxy Casting Compound
Tra-Con Tra-Bond 2222 One-Part Surface Mount Epoxy Adhesive
Tra-Con Tra-Bond 2143D Medium Viscosity Polyamide Epoxy Adhesive

PLORD039 / 86047

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.