MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Go Yen Chemical GYC DINP Di-lsononyl Phthalate
Categories: Other Engineering Material

Material Notes: GYC DINP (Di-lsononyl Phthalate) is produced by esterifying Isononanol and Phthalic Anhydride.

Introduction:

  • its plasticizing efficiency, migration and water extraction rate are lower and its gelation temperature and electric resistivity are mildly higher.
  • DINP’s low volatility not only prolongs the service life of product but also reduces the evaporation during process.
  • the plasticizing efficiency and specific gravity is higher, to save a considerable cost per volume. poisonless,
  • it’s suitable for foodstuffs wrapping, toys and plastic inflation products.< /ul>Usage:
    • Wires & Cables
    • Leather & Clothes
    • Gloves
    • Shoes
    • Construction materials
    • Poisonless plastic products
    • Food wrapping, toys and plastic inflation products
    • PVC plastisols etc

    Information provided by Go Yen Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.969 - 0.979 g/cc0.0350 - 0.0354 lb/in³(20/20)
Viscosity 45 cP
@Temperature 30.0 °C
45 cP
@Temperature 86.0 °F
Molecular Weight 419 g/mol419 g/mol
 
Chemical PropertiesMetricEnglishComments
Acid Value <= 0.050<= 0.050[mgKOH/g]
 
Thermal PropertiesMetricEnglishComments
Melting Point -50.0 °C-58.0 °FFreezing point
Boiling Point 403 °C
@Pressure 0.101 MPa
757 °F
@Pressure 14.7 psi
Flash Point 213 °C415 °F
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.481 - 1.4871.481 - 1.487
 
Descriptive Properties
Color<25APHA
Heat loss<0.1125°Cx3hr
Properties262-272 mgkOH/gEsterification number

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PGOYEN902 / 267210

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.