MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

RESPOL EBANTIX® E1770 EBA
Categories: Polymer; Thermoplastic; Ethylene Butyl Acrylate

Material Notes: Product Description: EBA REPSOL EBANTIX® E1770 is a copolymer suitable for general extrusion, injection molding and compounds where good processability, flexibility and very good mechanical properties are required. The butyl acrylate content is 17%. It contains antioxidant additives.
Applications: Extrusion (profiles, sheets); Injection molding; Microcellular foams; Compounds and masterbatches; Cables
Recommended melt temperature 180°C. EBA copolymers exhibit excellent thermal stability, which allows higher processing temperatures if needed. Processing characteristics of E1770 are similar to LDPE and conventional polyethylene extruders are recommended. Processing conditions should be optimized for each production line.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Additive: Antioxidant

Features: Antioxidant; Copolymer, Food Contact Acceptable; Good Flexibility; Good Processability

Uses: Compounding; Foam; Profiles; Sheet

Agency Ratings: EU Food Contact

Processing Method: Compounding; Extrusion; Injection Molding

Information provided by REPSOL

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.924 g/cc0.0334 lb/in³ISO 1183
Butyl Acrylate Content 17 %17 %
Melt Flow 7.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
7.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9090ISO 868
Hardness, Shore D 3131ISO 868
Tensile Strength at Break 12.0 MPa1740 psiISO 527-2
Film Elongation at Break, MD 800 %800 %ISO 527-2
Film Elongation at Break, TD 800 %800 %ISO 527-2
 
Thermal PropertiesMetricEnglishComments
Melting Point 92.8 °C199 °F
Vicat Softening Point 61.1 °C142 °FISO 306/A
 
Processing PropertiesMetricEnglishComments
Melt Temperature 180 °C356 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PRESPOL1309 / 312002

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.