MetalTek MTEK WC 1 UNS J13047 Cast Alloy Steel
Categories:
Metal
;
Ferrous Metal
;
Alloy Steel
;
AISI 8000 Series Steel
Material Notes:
General structural use.
Applications: Cylinders, rolls, hollow shafts.
Information provided by MetalTek
Key Words:
Cast UNS J13047; Cast Grade A4; Cast ASTM A217; Wrought UNS G86200; Wrought Grade AISI 8620
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Mechanical Properties
Metric
English
Comments
Hardness, Brinell
197
197
Tensile Strength, Ultimate
>=
450
MPa
>=
65300
psi
Tensile Strength, Yield
>=
240
MPa
>=
34800
psi
Elongation at Break
>= 24 %
>= 24 %
Component Elements Properties
Metric
English
Comments
Carbon, C
<= 0.25 %
<= 0.25 %
Iron, Fe
97.7 - 99.05 %
97.7 - 99.05 %
As Balance
Manganese, Mn
0.50 - 0.80 %
0.50 - 0.80 %
Molybdenum, Mo
0.45 - 0.65 %
0.45 - 0.65 %
Silicon, Si
<= 0.60 %
<= 0.60 %
Descriptive Properties
Heat Treatment
Quench & Temper
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
MetalTek MTEK 221-01 Cast UNS J84090 Martensitic Stainless Steel
MetalTek WC 6 Cast UNS J24054 Alloy Steel
MetalTek MTEK WC 9 Cast UNS J42045 Alloy Steel
MetalTek WCB UNS J13345 Cast Alloy Steel
Crucible Steel AISI 8620 Alloy Steel
NMETEK116 / 18366
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.