MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Chemical Concepts Chem-Set™ 605 Quick Set Acrylic Adhesive
Categories: Polymer; Adhesive; Thermoset; Acrylic/Cyanoacrylate Adhesive

Material Notes: ChemSet 605 Quick Set Acrylic Adhesive is a toughened structural adhesive that after curing, produces superior strength load-bearing bonds to engineered plastics including under mount sink anchors for solid surface, engineered stone and quartz. ChemSet 605 also bonds to PVC, fiberglass, ABS, FRT, PPO, PCBB, Metton®, Lomod®, Valox®, Noryl®, GTX, Minlon®, epoxy, RIM urethane, wood, poorly prepared surfaces, and where outdoor weathering or solvent exposure is anticipated. Features: Minimal surface preparation. Room temperature cure. 1:1 mix ratio. Rapid fixture in thin set Non-sagging formula.

Information provided by Chemical Concepts™.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.28 lb/galmixed
Viscosity 50000 cPTB @ 10 rpm, Activator, uncured
 55000 cPTB @ 10 rpm, Adhesive, uncured
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 78cured
Elongation at Break 15 - 25 %cured
Shear Strength 1300 psiABS, cured, stock failure; ASTM D1002
 1400 psiPolycarbonate Alloy, cured, stock failure; ASTM D1002
 3000 psiGrit blasted steel, cured; ASTM D1002
Peel Strength 35.0 - 40.0 plicured, 10"/min on 0.060" 6061 Aluminum; ASTM D1876
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 250 °FCured. Intermittent.
Minimum Service Temperature, Air -67.0 °Fcured
Flash Point 51.0 °Funcured
 
Processing PropertiesOriginal ValueComments
Cure Time 0.750 - 1.00 hourFunctional Cure
 
Descriptive Properties
Chemical Resistance8.11 lbs/gal, Activator, uncured
 8.44 lbs/gal, Adhesive, uncured
Coloroff white, Activator, uncured
 off white, Adhesive, uncured
Fixture Time15 minutes @ 72°F, uncured
Gap Filling0.125 inches, cured
Impact Resistance22ft.lb/in., Sat D950-61, Tgrit blasted steel, cured.
Open Time3 minutes @ 72°F, uncured

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCHEMI915 / 232173

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.