MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Dover Chemical DOVERNOX D9411T A high performance phosphite blend with excellent cost/performance as a polymer stabilizer
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Dovernox D-9411T is a one to one blend of Doverphos S-9228T and Doverphos S-480. It is offered by 1057 to be used in various polymer formulations as an excellent cost/performance processing stabilizer.

Information provided by DoverChem

Key Words: CAS# 154862-43-8, CAS# 31570-04-4
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.20 g/cc
@Temperature 25.0 °C
1.20 g/cc
@Temperature 77.0 °F
 
Chemical PropertiesMetricEnglishComments
Total Acid Number <= 1.0<= 1.0[mgKOH/g]
 
Thermal PropertiesMetricEnglishComments
Melting Point 180 - 230 °C356 - 446 °F
 
Component Elements PropertiesMetricEnglishComments
Phosphorus, P 6.0 %6.0 %
 
Descriptive Properties
AppearanceWhite/Off-White free-flowing granular
Component, % by weight50Doverphos S9228T
 50Doverphos S480, tris (2,4-di-t-butylphenyl) Phosphite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WDOVER064 / 217683

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.