MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Akrochem Antioxidant DLTDP
Categories: Other Engineering Material

Material Notes: Product Description: Antioxidant DLTDP is a thioether antioxidant synergist heat stabilizer. DLTDP find application where improved long-term, heat aging properties are required. Typically, DLTDP is used in conjunction with hindered phenolic antioxidants as well other antioxidant chemistries, to enhance their performance. It is a nonvolatile stabilizer and offers low oral and dermal toxicity. DLTDP is non-staining, with good color retention, good compatibility and low extractability. DLTDP can be use in peroxide cured elastomers as it has a minimal effect on vulcanization properties.

Application: Antioxidant DLTDP finds application in plastics, rubber, coatings and adhesives. In rubber, Antioxidant DLTDP can be used in SBR, NR-IR, EPR, EPDM, PBR, CR, NBR, and many other synthetic polymers. For superior heat stability, a synergistic ratio of three to one should be employed: DLTDP to hindered phenolic antioxidant. The typical dosage for rubber applications is 0.5 - 1.0 PHR (DLTDP) to 0.15-0.35 PHR (AO 1010, 1076, etc.). Antioxidant DLTDP is very effective in PP, ABS, and HDPE. Antioxidant DLTDP is listed as dilaurylthiodipropionate, and as such complies with 21 CFR 175.300 (Resinous and polymeric coatings) and CFR 177.2600 (Rubber articles intended for repeated use). Always verify current regulatory standards and dosage limitations for your specific application.

Information provided by Akrochem Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.920 g/cc
Volatiles <= 0.50 %
Ash <= 0.10 %
 
Thermal PropertiesOriginal ValueComments
Melting Point >= 39.0 °C
 
Descriptive Properties
Appearancewhite powder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PAKZCH491 / 315409

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.