Description: TIPPLEN R 665 XClear is a random copolymer polypropylene for extrusion. This improved grade is formulated with a new generation clarifying agent, so the product shows excellent optical properties (transparency and gloss). Applications: TIPPLEN R 665 XClear is recommended for blow molded bottles for detergents and toiletries. This grade is well suited for extruded sheet for stationery folder and thermoforming articles. (1) Average mechanical property values of several measurements carried out on standard injection-molded test specimens prepared in accordance with ISO 294-1. (2) Measured on specimen with 1 mm wall thickness Information provided by Molgroup Chemicals |