MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Eagle Brass 305 Austenitic Stainless Steel, Annealed
Categories: Metal; Ferrous Metal; Stainless Steel; T 300 Series Stainless Steel

Material Notes: Type 305 is a chromium nickel stainless steel that can be spun and deep drawn more easily due to an increased nickel content that decreases work hardening. It is nonmagnetic under most conditions. Typical uses include appliances, kitchen utensils, tank covers and other deep drawn parts.

Information provided by Eagle Brass Company

Key Words: ASTM A240; UNS S30500
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.286 lb/in³As Annealed
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength >= 70.0 ksi
Tensile Strength, Yield >= 25.0 ksi0.2% Offset
Elongation at Break >= 40 %in 2 inches
Tensile Modulus 28000 ksi
 
Thermal PropertiesOriginal ValueComments
CTE, linear 10.5 µin/in-°F
@Temperature 20.0 - 649 °C
Thermal Conductivity 107 BTU-in/hr-ft²-°F
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.12 %
Chromium, Cr 17 - 19 %
Iron, Fe 65.055 - 72.5 %Calculated as Balance
Manganese, Mn <= 2.0 %
Nickel, Ni 10.5 - 13 %
Phosphorus, P <= 0.045 %
Silicon, Si <= 0.75 %
Sulfur, S <= 0.030 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Eagle Brass 304 Austenitic Stainless Steel, Annealed
Eagle Brass 304L Austenitic Stainless Steel, Annealed
305 Stainless Steel, annealed, sheet
AISI Type 304L Stainless Steel
Eagle Brass 316 Austenitic Stainless Steel, 1/4 Hardened

NEAGLE531 / 147511

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.