MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Henkel Hysol EA 9390 Paste Adhesive System
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Low viscosity system for high temperature wet lay-up composite repair. Qualified to BMS 8-301.
    Applications:
  • Structural Bonding
  • Low Viscosity Wet Lay-Up
  • Composite Bonding

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Storage Temperature 4.00 °C
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 56.6 MPa
Elongation at Break 2.5 %
Tensile Modulus 2900 MPa
Compressive Strength 36.6 MPacompressive shear strength as a wet lay-up resin with 3K-70-P fiber
Adhesive Bond Strength 15.2 MPa
@Temperature -55.0 °C
Tensile Lap Shear
 20.7 MPa
@Temperature 93.0 °C
Tensile Lap Shear
 24.1 MPa
@Temperature 25.0 °C
Tensile Lap Shear
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air >= 177 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 3.50 hour
@Temperature 93.0 °C
Pot Life 120 min
 
Descriptive Properties
ConsistencyLow Viscosity
Form2 parts
Mix Ratio, Part A:Part B100:56
Peel StrengthNil

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Henkel Hysol EA 9360 Paste Adhesive System
Henkel Hysol EA 9394 Paste Adhesive System
Henkel Hysol EA 9320NA Paste Adhesive System
Henkel Hysol EA 934NA Paste Adhesive System
Henkel Hysol EA 9313 Paste Adhesive System

PHENK816 / 146821

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.