HCG2530MP is high rigidity and balance tenacity 30% GF PC resin. It has excellent surface, high NCVM rate, easy to machining , high stability and super shape resistance property. HCG2530MP is mainly used in mobile phone housing,Information provided by Shanghai Kumho Sunny Plastics co, Ltd |